Influence of two different heat treatment procedures on mechanical and fracture properties of 65Si7 steel


Pustaić, Dragan; Cajner, Franjo
Influence of two different heat treatment procedures on mechanical and fracture properties of 65Si7 steel // Advanced Materials and Technologies, AMT/2001 / Wittbrodt, Edmund (ur.).
Gdanjsk : Jurata: Sigma not, 2001. str. 733-736 (predavanje, međunarodna recenzija, cjeloviti rad (in extenso), znanstveni)


CROSBI ID: 89964 Za ispravke kontaktirajte CROSBI podršku putem web obrasca

Naslov
Influence of two different heat treatment procedures on mechanical and fracture properties of 65Si7 steel

Autori
Pustaić, Dragan ; Cajner, Franjo

Vrsta, podvrsta i kategorija rada
Radovi u zbornicima skupova, cjeloviti rad (in extenso), znanstveni

Izvornik
Advanced Materials and Technologies, AMT/2001 / Wittbrodt, Edmund - Gdanjsk : Jurata : Sigma not, 2001, 733-736

Skup
XVIth Physical Metallurgy and Materials Science Conference on Advanced Materials and Technologies, AMT/2001

Mjesto i datum
Gdańsk, Poljska; Jurata, Poljska, 16.09.2001. - 20.09.2001

Vrsta sudjelovanja
Predavanje

Vrsta recenzije
Međunarodna recenzija

Ključne riječi
Heat treatment; Steel 65Si7; Mechanical properties; Fracture mechanics parameters

Sažetak
This paper deals with the results of investigations of two different heat treatment procedures and their influence on some mechanical properties as well as on the magnitude of some fracture mechanics parameters for a particular type of steel. Experimental investigations were performed on the specimens made of 65 Si 7 steel. The processes occurring by tempering of two different microstructures of the steel, i. e. martensite and lower bainite were investigated. An advantage of austempering over hardening and tempering is in obtaining the bainite microstructure. Steel of bainite microstructure has a greater toughness, ductility, contraction, fatigue strength and a better fracture toughness than a tempered martensite of the same type of steel. A bainite microstructure also gives a better resistance to thermal fatigue in comparison with martensite microstructure. The above mentioned improved values of mechanical properties refer to the untempered state of bainite.

Izvorni jezik
Engleski

Znanstvena područja
Strojarstvo



POVEZANOST RADA


Projekti:
120091

Ustanove:
Fakultet strojarstva i brodogradnje, Zagreb

Profili:

Avatar Url Franjo Cajner (autor)

Avatar Url Dragan Pustaić (autor)


Citiraj ovu publikaciju:

Pustaić, Dragan; Cajner, Franjo
Influence of two different heat treatment procedures on mechanical and fracture properties of 65Si7 steel // Advanced Materials and Technologies, AMT/2001 / Wittbrodt, Edmund (ur.).
Gdanjsk : Jurata: Sigma not, 2001. str. 733-736 (predavanje, međunarodna recenzija, cjeloviti rad (in extenso), znanstveni)
Pustaić, D. & Cajner, F. (2001) Influence of two different heat treatment procedures on mechanical and fracture properties of 65Si7 steel. U: Wittbrodt, E. (ur.)Advanced Materials and Technologies, AMT/2001.
@article{article, author = {Pustai\'{c}, Dragan and Cajner, Franjo}, editor = {Wittbrodt, E.}, year = {2001}, pages = {733-736}, keywords = {Heat treatment, Steel 65Si7, Mechanical properties, Fracture mechanics parameters}, title = {Influence of two different heat treatment procedures on mechanical and fracture properties of 65Si7 steel}, keyword = {Heat treatment, Steel 65Si7, Mechanical properties, Fracture mechanics parameters}, publisher = {Sigma not}, publisherplace = {Gda\'{n}sk, Poljska; Jurata, Poljska} }
@article{article, author = {Pustai\'{c}, Dragan and Cajner, Franjo}, editor = {Wittbrodt, E.}, year = {2001}, pages = {733-736}, keywords = {Heat treatment, Steel 65Si7, Mechanical properties, Fracture mechanics parameters}, title = {Influence of two different heat treatment procedures on mechanical and fracture properties of 65Si7 steel}, keyword = {Heat treatment, Steel 65Si7, Mechanical properties, Fracture mechanics parameters}, publisher = {Sigma not}, publisherplace = {Gda\'{n}sk, Poljska; Jurata, Poljska} }




Contrast
Increase Font
Decrease Font
Dyslexic Font