Grooving corrosion of welded galvanize pipes for distribution of warm water
Grooving corrosion of welded galvanize pipes for distribution of warm water // Corrosion Control in the Service of Society
Las Vegas (NV): NACE International, 2008. (predavanje, međunarodna recenzija, cjeloviti rad (in extenso), znanstveni)
CROSBI ID: 404068 Za ispravke kontaktirajte CROSBI podršku putem web obrasca
Naslov
Grooving corrosion of welded galvanize pipes for distribution of warm water
Autori
Esih, Ivan ; Juraga, Ivan ; Šimunović, Vinko ; Alar, Vesna ; Stojanović, Ivan
Vrsta, podvrsta i kategorija rada
Radovi u zbornicima skupova, cjeloviti rad (in extenso), znanstveni
Izvornik
Corrosion Control in the Service of Society
/ - Las Vegas (NV) : NACE International, 2008
Skup
17th International Corrosion Congress
Mjesto i datum
Las Vegas (NV), Sjedinjene Američke Države, 06.10.2008. - 10.10.2008
Vrsta sudjelovanja
Predavanje
Vrsta recenzije
Međunarodna recenzija
Ključne riječi
grooving corrosion; galvanized pipes; warm water
(grooving corrosion; galvanized pipes; warm water.)
Sažetak
Premature failure of galvanized pipes in the distribution network of a facility supplying numerous consumers with warm water has taken place. It was caused by grooving corrosion of longitudinal weldments resulting in intensive leakage of the system. Detailed analysis of the facility and of the way of its operation was carried out using various techniques. The analysis comprised physical and chemical data on - fresh water, - structural materials and - corrosion process and its products. It was established that the water in the network is contaminated with Cu2+ brought into existence by corrosion of copper pipes used in the central heater of the system. On the other hand the temperature of water is approximately 70 oC when the network is in operation. Under such circumstances significant changes of open circuit potentials of zinc and steel take place, influencing the corrosion behavior of the investigated system. Simultaneously, copper is deposited on galvanized steel by ionic replacement that makes possible intensive bimetallic corrosion localized on longitudinal weldments.
Izvorni jezik
Engleski
Znanstvena područja
Strojarstvo
POVEZANOST RADA
Projekti:
120-1201767-1764 - Lokalni korozijski fenomeni na nehrđajućih čelicima i njihovo sprečavanje (Juraga, Ivan, MZOS ) ( CroRIS)
152-1521473-1475 - Povećanje učinkovitosti i kvalitete odljevaka-hrvatske perspektive (Budić, Ivan, MZOS ) ( CroRIS)
Ustanove:
Fakultet strojarstva i brodogradnje, Zagreb
Profili:
Vinko Šimunović
(autor)
Ivan Esih
(autor)
Ivan Juraga
(autor)
Ivan Stojanović
(autor)
Vesna Alar
(autor)