Pregled bibliografske jedinice broj: 293899
Stress-Strain Analysis of Single-lap Tensile Loaded Adhesive Joints
Stress-Strain Analysis of Single-lap Tensile Loaded Adhesive Joints // CP908, NUMIFORM '07, Materials, Processing and Design: Modeling, Simulation and Applications. / César de Sá, J.M.A. ; Santos, A.D. (ur.).
Porto: American Institute of Physics (AIP), 2007. str. 1093-1098 (predavanje, međunarodna recenzija, cjeloviti rad (in extenso), znanstveni)
CROSBI ID: 293899 Za ispravke kontaktirajte CROSBI podršku putem web obrasca
Naslov
Stress-Strain Analysis of Single-lap Tensile Loaded Adhesive Joints
Autori
Raos, Pero ; Kozak, Dražan ; Lucić, Mirjana
Vrsta, podvrsta i kategorija rada
Radovi u zbornicima skupova, cjeloviti rad (in extenso), znanstveni
Izvornik
CP908, NUMIFORM '07, Materials, Processing and Design: Modeling, Simulation and Applications.
/ César de Sá, J.M.A. ; Santos, A.D. - Porto : American Institute of Physics (AIP), 2007, 1093-1098
ISBN
978-0-7354-0416-8
Skup
The 9th Int. Conference on Numerical Methods in Industrial Forming Processes NUMIFORM '07
Mjesto i datum
Porto, Portugal, 17.06.2007. - 21.06.2007
Vrsta sudjelovanja
Predavanje
Vrsta recenzije
Međunarodna recenzija
Ključne riječi
Single-Lap Adhesive Joints; Tensile Loading; Experiment; Finite Element Analysis; Optimal Overlap Length
Sažetak
Both, experimental investigation and finite element analysis of single-lap adhesive joints subjected to tension have been done to find out an optimal overlap length. As the adherend material aluminum was considered with the two component high-strength engineering adhesive for the bonding of the layers. The thickness of the sheet metal layer was 1, 95 mm, while adhesive was 0, 15 mm thick. The width of all thin plates was 30 mm, but the overlap length varied as 15, 20, 30, 40 and 60 mm. Real mechanical properties of all materials in the joint have been determined experimentally. Obtained results proved that the overlap length affects directly the joint tensile strength, where an optimum value of overlap length can be defined. Finite element analysis of stress and strain fields could help to determine the moment when the crack failure spreads from overlap ends to the inside. In such a manner it could be better understand complex mechanisms of failure of adhesive joints.
Izvorni jezik
Engleski
Znanstvena područja
Strojarstvo
POVEZANOST RADA
Projekti:
152-1201910-1909 - Analiza i procjena loma konstrukcija iz anizotropnih materijala (Kozak, Dražan, MZOS ) ( CroRIS)
152-1521473-1474 - Napredni postupci izravne izradbe polimernih proizvoda (Raos, Pero, MZOS ) ( CroRIS)
152-1521473-1476 - Suvremene tehnologije spajanja lakih strojarskih konstrukcija (Samardžić, Ivan, MZOS ) ( CroRIS)
152-1521473-3111 - Značajke proizvoda za sveukupnu realizaciju proizvoda kod brze proizvodnje (Kljajin, Milan, MZOS ) ( CroRIS)
Ustanove:
Strojarski fakultet, Slavonski Brod