Pregled bibliografske jedinice broj: 255843
Carbamide-formaldehyde adhesive systems modified with liquefied wood Part I. Acid catalyst method of wood liquefaction with various polyhydric alcohols
Carbamide-formaldehyde adhesive systems modified with liquefied wood Part I. Acid catalyst method of wood liquefaction with various polyhydric alcohols // Technologies of wood processing / Klement, Ivan (ur.).
Zvolen: Technical University in Zvolen, Faculty of Wood Science and Technology, 2006. str. 7 - 14 (predavanje, međunarodna recenzija, cjeloviti rad (in extenso), znanstveni)
CROSBI ID: 255843 Za ispravke kontaktirajte CROSBI podršku putem web obrasca
Naslov
Carbamide-formaldehyde adhesive systems modified with liquefied wood Part I. Acid catalyst method of wood liquefaction with various polyhydric alcohols
Autori
Antonović, Alan ; Kunaver, Matjaž ; Jambreković, Vladimir ; Kržan, Andrej ; Pervan, Stjepan, Ištvanić, Josip
Vrsta, podvrsta i kategorija rada
Radovi u zbornicima skupova, cjeloviti rad (in extenso), znanstveni
Izvornik
Technologies of wood processing
/ Klement, Ivan - Zvolen : Technical University in Zvolen, Faculty of Wood Science and Technology, 2006, 7 - 14
Skup
Technologies of wood processing
Mjesto i datum
Zvolen, Slovačka, 19.09.2006. - 20.09.2006
Vrsta sudjelovanja
Predavanje
Vrsta recenzije
Međunarodna recenzija
Ključne riječi
liquefied wood; polyhydric alcohols; acid catalyst; undissolved residue; hydroxyl number
Sažetak
Wood liquefaction of black poplar (Populus nigra L.) with various polyhidric alcohols through acid catalyst method was studied for the purposes of determination the best polymer characteristics of liquefied wood, as a further raw material in modified carbamide-formaldehyde resin synthesis, with respect to adhesives in wood based panels production. For liquefaction we used several types of polyhidric alcohols (PEG, DEG, DPG, EG and glycerol) and H2SO4 as acid catalyst under defined conditions of liquefaction reaction: wood/liquefaction reagent/H2SO4 = 20.00/112.45/3.37 gram, at 150 °C for 120 min. For various liquefaction reagents mixtures of polyhidric alcohols, undissolved residue percentage (0.50-5.69%), and hydroxyl OH-number (88-567 mg KOH/g) was provide as a value which determine liquefied wood polymer characteristics. The best effects were achived using mixtures of glycerol/DEG/H2SO4 (80/20/3) and glycerol/ H2SO4 (100/3).
Izvorni jezik
Engleski
Znanstvena područja
Šumarstvo
POVEZANOST RADA
Projekti:
0068137
Ustanove:
Fakultet šumarstva i drvne tehnologije
Profili:
Stjepan Pervan
(autor)
Josip Ištvanić
(autor)
Vladimir Jambreković
(autor)
Alan Antonović
(autor)