Pregled bibliografske jedinice broj: 140667
Motional heterogeneity of polystyrene-block-polybutadiene: a spin probe study
Motional heterogeneity of polystyrene-block-polybutadiene: a spin probe study // Polymer, 44 (2003), 26; 7875-7881 doi:10.1016/j.polymer.2003.10.023 (međunarodna recenzija, članak, znanstveni)
CROSBI ID: 140667 Za ispravke kontaktirajte CROSBI podršku putem web obrasca
Naslov
Motional heterogeneity of polystyrene-block-polybutadiene: a spin probe study
Autori
Čulin, Jelena ; Andreis, Mladen ; Veksli, Zorica ; Gallot, Yves
Izvornik
Polymer (0032-3861) 44
(2003), 26;
7875-7881
Vrsta, podvrsta i kategorija rada
Radovi u časopisima, članak, znanstveni
Ključne riječi
ESR ; Spin probes ; Heterogeneity ; Block copolymers
Sažetak
Polystyrene-block-polybutadiene copolymers (SB) with 0.5 mass fraction of styrene were studied by electron spin resonance (ESR) of nitroxide spin probes. The influence of the block length ( = 12000, = 48000 and = 83000) and the solvation power of casting solvents on the motional dynamics of spin probe were measured over a wide temperature range. Two nitroxide radicals as spin probes were selected: 2, 2, 6, 6-tetramethyl-4-hydroxypiperidine-1-oxyl benzoate (BzONO) and 2, 2, 6, 6-tetramethyl-4-hydroxypiperidine-1-oxyl (Tempol). Irrespective of the spin probe used two ESR spectral components differing in their motional properties above the phase transition of polybutadiene blocks (PB) were observed. The fast component was assigned to spin probes located in polybutadiene-rich domains and the slow component to spin probes in polystyrene- rich domains. The range of two spectral components and the phase transition of the slow ESR component, T5mT, depend on the block length. The influence of the interphase and accumulation of free volume in the interphase on the Tempol probe motion was investigated by changing copolymer morphology in the films casted from selective and nonselective solvents. The analysis of the motional heterogeneity from the ratio of the fast and slow motional component presents evidence that in the selective solvent for polystyrene (PS) blocks (2-butanone) the most irregular structure with a large interphase is formed. The difference in fast motion of spin probes indicates that the motional dynamic is related to the change of domain structure.
Izvorni jezik
Engleski
Znanstvena područja
Kemija
Citiraj ovu publikaciju:
Časopis indeksira:
- Current Contents Connect (CCC)
- Web of Science Core Collection (WoSCC)
- Science Citation Index Expanded (SCI-EXP)
- SCI-EXP, SSCI i/ili A&HCI
- Scopus