Pregled bibliografske jedinice broj: 89875
Određivnje kemijske stabilnosti dentalne keramike u kiselom mediju metodama spektrofotometrije i ionske kromatografije
Jakovac, M., Živko-Babić, J., Ćurković, L., Pandurić, J. & Jerolimov, V. (2002) Određivnje kemijske stabilnosti dentalne keramike u kiselom mediju metodama spektrofotometrije i ionske kromatografije. Acta Stomatologica Croatica, 36 (1), 85-96.
CROSBI ID: 89875 Za ispravke kontaktirajte CROSBI podršku putem web obrasca
Naslov
Određivnje kemijske stabilnosti dentalne keramike u kiselom mediju metodama spektrofotometrije i ionske kromatografije
(Application of Spectrophotometricy and Ion Chromatography for Monitoring the Chemical Stability of Dental Ceramics in Acid Solution)
Autori
Jakovac, Marko ; Živko-Babić, Jasenka ; Ćurković, Lidija ; Pandurić, Josip ; Jerolimov, Vjekoslav
Izvornik
Acta Stomatologica Croatica (0001-7019) 36
(2002), 1;
85-96
Vrsta, podvrsta i kategorija rada
Radovi u časopisima, članak, znanstveni
Ključne riječi
Kemijska stabilnost; dentalna keramika; ionska kromatografija
(chemical stability; dental ceramics; ion chromatography)
Sažetak
The corrosive process of dental alloy is well known, although little information is available on the corrosion of dental ceramics. The aim of this study was the analysis of the cmenical stability of two dental ceramics in an aggresive medium. Two samples of feldspatic ceramics in an aggressive medium. Two samples of feldspatic ceramic fused to Co-Cr and Ni-Cr alloy and a sample of hydrothermal ceramic fused to highnobel gold alloy were deposited in 10-3 mol/L HCl at 50 oC during six months. The solutions were analysed after one, two, three and six months. The determination of Na+, K+, Ca2+ and Mg2+ was performed by ion chromatographiy (IC), the quantities of eluted Si4+ and Al3+ were determined by spectrophotometric method and the wihgt loss of each sample was measured by analytical scale. The changes of the pH values were determined by menas of a pH meter. The results showed that most ions were eluted after the first three moinths, while after that period of time elution was significantly lower in each sample. The sample with hydrothermal ceramic showed the most significant elutio and the highest weight loss. The pH values changed in each leachate sample, but stabilised after the 3rd month of the investigation. It can be concluded that dental ceramics are not stable in an acid medium.
Izvorni jezik
Hrvatski, engleski
Znanstvena područja
Strojarstvo, Dentalna medicina
POVEZANOST RADA
Ustanove:
Stomatološki fakultet, Zagreb,
Fakultet strojarstva i brodogradnje, Zagreb
Profili:
Lidija Ćurković
(autor)
Jasenka Živko-Babić
(autor)
Vjekoslav Jerolimov
(autor)
Marko Jakovac
(autor)
Josip Pandurić
(autor)