Pregled bibliografske jedinice broj: 301378
Lubricating film formation for strip dressing
Lubricating film formation for strip dressing // Goriva i maziva, 46 (2007), 1; 34-44 (recenziran, članak, znanstveni)
CROSBI ID: 301378 Za ispravke kontaktirajte CROSBI podršku putem web obrasca
Naslov
Lubricating film formation for strip dressing
Autori
Ćurčija, Dušan ; Mamuzić, Ilija
Izvornik
Goriva i maziva (0350-350X) 46
(2007), 1;
34-44
Vrsta, podvrsta i kategorija rada
Radovi u časopisima, članak, znanstveni
Ključne riječi
lubricating film ; strip ; Monte-Carlo method ; dressing
Sažetak
The geometrical lubricating film formation on a strip in front of the rollers at dressing process is analyzed. The effect of the initial thickness of the lubricant film on the initial section of the metal deformation zone is calculated. This effect is great for low rolls gripping angle. The differential equation for extreme geometrical properties of the lubricating layerin before the initial section of the deformation zone is solved by the Monte- Carlo method. This geometry can be achieved in dressing processes using high quality lubricants, aimed to save lubricant in the technological process. In the series of diagrams the critical point separating the optimal thickness of the lubricant film from the excess of lubricant is established. For theoretical investigations, the positioning of this critical point is of essential importance.
Izvorni jezik
Engleski
Znanstvena područja
Metalurgija
POVEZANOST RADA
Projekti:
120-1201787-1491 - Oblikovanje deformiranjem i svojstva novih metalnih materijala (Mamuzić, Ilija, MZOS ) ( CroRIS)
124-1241565-1537 - Struktura, svojstva i separacija metalnih materijala (Matković, Tanja, MZOS ) ( CroRIS)
Ustanove:
Metalurški fakultet, Sisak
Citiraj ovu publikaciju:
Uključenost u ostale bibliografske baze podataka::
- Chemical Engineering and Biotechnology Abstracts
- TRIS (Transport Res)