Pregled bibliografske jedinice broj: 1259797
Corrosion of cold isostatic pressed alumina ceramics
Corrosion of cold isostatic pressed alumina ceramics // INTERNATIONAL CONFERENCE ON NEW ACHIEVEMENTS IN SCIENCE, TECHNOLOGY AND ARTS ICNA-STA / Gallopeni, Bujar ; Shehu, Alma ; Adnan, Lataj ; Gashi, Damir (ur.).
Peja: International Business College Mitrovica (IBC-M) ; University Haxhi Zeka Peja ; South East European University, Skopje, North Macedonia, 2022. str. 113-113 (poster, međunarodna recenzija, sažetak, znanstveni)
CROSBI ID: 1259797 Za ispravke kontaktirajte CROSBI podršku putem web obrasca
Naslov
Corrosion of cold isostatic pressed alumina
ceramics
Autori
Ćurković, Lidija ; Ropuš, Ivana ; Rončević, Sanda ; Veseli, Rea
Vrsta, podvrsta i kategorija rada
Sažeci sa skupova, sažetak, znanstveni
Izvornik
INTERNATIONAL CONFERENCE ON NEW ACHIEVEMENTS IN SCIENCE, TECHNOLOGY AND ARTS ICNA-STA
/ Gallopeni, Bujar ; Shehu, Alma ; Adnan, Lataj ; Gashi, Damir - Peja : International Business College Mitrovica (IBC-M) ; University Haxhi Zeka Peja ; South East European University, Skopje, North Macedonia, 2022, 113-113
ISBN
978-9951-9090-0-6
Skup
INTERNATIONAL CONFERENCE ON NEW ACHIEVEMENTS IN SCIENCE, TECHNOLOGY AND ARTS ICNA-STA
Mjesto i datum
Peja, Kosovo, 14.04.2022. - 15.04.2022
Vrsta sudjelovanja
Poster
Vrsta recenzije
Međunarodna recenzija
Ključne riječi
highly pure alumina ; ion elution ; inductively coupled plasma atomic emission spectrometry ; corrosion kinetics
Sažetak
Aluminum oxide (Al2O3) or alumina, like most ceramic materials, can withstand harsh environments. In order to measure the corrosion resistance of cold isostatic pressed (CIP) high purity alumina, its dissolution in aqueous nitric acid (HNO3) solutions was studied as a function of immersion time and acid concentration. The corrosion resistance of CIP Al2O3 was investigated in the following concentrations of HNO3: 0.5, 1.25 and 2 mol dm-3 at temperatures of 25, 40 and 55 °C and with an exposure time of up to 240 h. The number of eluted ions (Al3+, Ca2+, Fe3+, Mg2+, Na+ and Si4+) was measured by inductively coupled plasma atomic emission spectrometry (ICP-AES). Furthermore, corrosion rate constants were determined. The corrosion resistance of the investigated highly pure alumina slightly decreased with an increase of nitric acid concentration. Nevertheless, very low dissolution values of Al3+, Ca2+, Fe3+, Mg2+, Na+ and Si4+ions after the corrosion test showed a very good corrosion resistance of alumina ceramics to the HNO3 aqueous solutions.
Izvorni jezik
Engleski
Znanstvena područja
Kemijsko inženjerstvo, Strojarstvo, Temeljne tehničke znanosti
POVEZANOST RADA
Projekti:
HRZZ-IP-2016-06-6000 - Napredna monolitna i kompozitna keramika za zaštitu od trošenja i korozije (WECOR) (Ćurković, Lidija, HRZZ - 2016-06) ( CroRIS)
Ustanove:
Prirodoslovno-matematički fakultet, Zagreb