Pregled bibliografske jedinice broj: 1249544
Effects of ambient exposure on photoluminescence of Dion-Jacobson tin-based halide perovskite
Effects of ambient exposure on photoluminescence of Dion-Jacobson tin-based halide perovskite // Journal of Materials Chemistry C, 11 (2023), 2737-2747 doi:10.1039/d2tc04912k (međunarodna recenzija, članak, znanstveni)
CROSBI ID: 1249544 Za ispravke kontaktirajte CROSBI podršku putem web obrasca
Naslov
Effects of ambient exposure on photoluminescence of
Dion-Jacobson tin-based halide perovskite
Autori
Sun, Wenting ; Xing, zengshan ; Sergeev, Aleksandr A. ; He, Yanlin ; Ng, Alan Man Ching ; Wong, Kam Sing ; Molčanov, Lidija ; Popović, Jasminka ; Djurisic, Aleksandra
Izvornik
Journal of Materials Chemistry C (2050-7526) 11
(2023);
2737-2747
Vrsta, podvrsta i kategorija rada
Radovi u časopisima, članak, znanstveni
Ključne riječi
Dion-Jacobson ; tin-based halide perovskite
Sažetak
Tin-based halide perovskite materials are of interest for light-emitting applications due to their broad yellow emission, but they are known to exhibit inferior stability compared to the lead- based perovskites due to tendency of Sn2+ to be readily oxidized. Here we investigated the ambient stability of a Dion-Jacobson tin bromide perovskite. We found that the optical properties of the samples were more significantly affected by the moisture rather than the ratio of Sn2+/Sn4+. The exposure to humidity resulted in changes in the ratio of 2D HDASnBr4 and hydrated 1D HDA3SnBr8 phases, with initial increase (up to ~40 h) in luminescence attributed to increasing fraction of hydrated 1D phase which contributes to self- trapped exciton emission. With further exposure to humidity, the material starts to degrade resulting in reduced luminescence after ~40 h. The use of additives for the suppression of oxidation of Sn2+, namely SnCl2 and tetraethyl orthosilicate (TEOS), results in prolonging the lifetime of the samples (>260 h for thin films with additives, compared to 180 h for thin films without additives). However, the persistence of luminescence with increased time of ambient exposure in samples prepared with additives can be attributed to the changes in the evolution of phase composition (rati-os of 2D and hydrated 1D phases) over time rather than suppressing the oxidation of Sn2+.
Izvorni jezik
Engleski
Znanstvena područja
Fizika, Kemija
POVEZANOST RADA
Projekti:
HRZZ-PZS-2019-02-2068 - 2D i kvazi-2D perovskiti: od ciljanog strukturnog dizajna do poboljšane učinkovitosti i stabilnosti (Popović, Jasminka, HRZZ - 2019-02) ( CroRIS)
Ustanove:
Institut "Ruđer Bošković", Zagreb
Citiraj ovu publikaciju:
Časopis indeksira:
- Current Contents Connect (CCC)
- Web of Science Core Collection (WoSCC)
- Science Citation Index Expanded (SCI-EXP)
- SCI-EXP, SSCI i/ili A&HCI
- Scopus