Pregled bibliografske jedinice broj: 1008064
Scaling features of conductivity spectra reveal complexities in ionic, polaronic and mixed ionic-polaronic conduction in phosphate glasses
Scaling features of conductivity spectra reveal complexities in ionic, polaronic and mixed ionic-polaronic conduction in phosphate glasses // Acta materialia, 175 (2019), 46-54 doi:10.1016/j.actamat.2019.05.067 (međunarodna recenzija, članak, znanstveni)
CROSBI ID: 1008064 Za ispravke kontaktirajte CROSBI podršku putem web obrasca
Naslov
Scaling features of conductivity spectra reveal complexities in ionic, polaronic and mixed ionic-polaronic conduction in phosphate glasses
Autori
Šantić, Ana ; Nikolić, Juraj ; Pavić, Luka ; Banhatti, Radha D. ; Mošner, Petr ; Koudelka, Ladislav ; Moguš-Milanković, Andrea
Izvornik
Acta materialia (1359-6454) 175
(2019);
46-54
Vrsta, podvrsta i kategorija rada
Radovi u časopisima, članak, znanstveni
Ključne riječi
Electrical conductivity ; Ionic diffusion ; Polaron ; Impedance spectroscopy ; Phosphate glasses ; Structure–property relationship
Sažetak
The scaling behaviour of six series of mixed ion-polaron glasses with the composition xWO3/MoO3-(30–0.5x)Li2O/Na2O/Ag2O-(30–0.5x)ZnO- 40P2O5, 0 ≤ x ≤ 60 mol%, has been studied using Summerfield and Sidebottom scaling procedures that are model free. The validity of the Sidebottom scaling procedure for each individual glass confirms that all glasses obey time-temperature superposition principle implying that the conduction mechanism does not change with temperature. On the other hand, Summerfield scaling is not found valid for all glasses. First, this deviation is observed in all glasses containing Li2O up to 20 mol% of MoO3/WO3. We relate this result to a non- typical interaction of Li+ ion with the compact zinc phosphate network resulting either in change of its hopping distance or in available conduction pathways for it as a function of temperature. Second, non-Summerfield scaling was also observed for glasses containing Li2O/Na2O/Ag2O with about 30 to 40 mol% of WO3. Thus, the origin of this deviation lies in the significant amounts of both types of charge carriers - ions and polarons, and their differently thermally activated mobilities.
Izvorni jezik
Engleski
Znanstvena područja
Fizika, Kemija
POVEZANOST RADA
Projekti:
IP-2014-09-5863 - Električni transport u staklima i staklo-keramici (EL-Trass-Ceram) (Moguš-Milanković, Andrea, HRZZ - 2014-09) ( CroRIS)
Ustanove:
Institut "Ruđer Bošković", Zagreb
Profili:
Andrea Moguš-Milanković
(autor)
Juraj Nikolić
(autor)
Ana Šantić
(autor)
Luka Pavić
(autor)
Citiraj ovu publikaciju:
Časopis indeksira:
- Current Contents Connect (CCC)
- Web of Science Core Collection (WoSCC)
- Science Citation Index Expanded (SCI-EXP)
- SCI-EXP, SSCI i/ili A&HCI
- Scopus