Porosity of ceramic shell molds (CROSBI ID 675322)
Prilog sa skupa u zborniku | sažetak izlaganja sa skupa | međunarodna recenzija
Podaci o odgovornosti
Usenko, R. ; Bichevnik, I. ; Mamuzić, Ilija
engleski
Porosity of ceramic shell molds
It is established that the open porosity of the uncalcined (wet) ceramic shell mold on the basis of quartz sand and liquid glass is 12 ... 14% (by volume), after heating to 950-15 °C and cooling with oven to 20... 25 °C - 18 ... 27% (by volume). The increase in porosity in the calcined ceramic shell mold is due to the appearance in it of new capillary channels. The appearance of such capillary channels is caused by thermal expansion-compression of the material of the mold during its heating and subsequent cooling.
porosity ; ceramic shell molds ; thermal expansion-compression
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
Podaci o prilogu
214-214.
2018.
objavljeno
Podaci o matičnoj publikaciji
13th International Symposium of Croatian Metallurgical Society "Materials and Metallurgy" SHMD 2018 : Book of Abstracts (tiskano u: Metalurgija 57 (2018) 3)
Mamuzić, Ilija
Zagreb: Hrvatsko metalurško društvo
Podaci o skupu
13th International Symposium of Croatian Metallurgical Society „Materials and Metallurgy“ (CMS) = 13. međunarodni simpozij Hrvatskog metalurškog društva (SHMD 2018) "Materijali i metalurgija"
poster
24.06.2018-29.06.2018
Šibenik, Hrvatska