The Study Conditions Occurrence of Hot Tearing in the Billets Alloy EN AW6060 Produced with the Process of Direct Chill Casting (CROSBI ID 643954)
Prilog sa skupa u zborniku | izvorni znanstveni rad | međunarodna recenzija
Podaci o odgovornosti
Buljeta, Ivica ; Beroš, Ana ; Zovko Brodarac, Zdenka
engleski
The Study Conditions Occurrence of Hot Tearing in the Billets Alloy EN AW6060 Produced with the Process of Direct Chill Casting
During Direct Chill casting of aluminum alloys technology Wagstaff AirSlip, the primary and secondary cooling causes strong thermal gradients, which leads to the uneven thermal contraction in different sections of the billet. The consequences are manifested appearance of casting defects such as hot tearing and residual stresses. In order to reduce the occurrence of these defects were studied different effects on the formation of hot tearing: changes of technological parameters, chemical composition and microstructure of the alloy EN AW 6060 according to the length and cross section, and the conditions of occurrence and progression of cracks describes the model the ratio of light and heavy metals in the billet. Additional testing of as - cast, cracked and homogenized sample billets in multiple directions cross- section detects that the rapid cooling of the surface of the billet affect the development of fields measured hardness.
Hot Tearing, Direct Chill Casting, Alloy EN AW6060
doi: 10.1002/9781119274780.ch113
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
Podaci o prilogu
673-678.
2016.
objavljeno
Podaci o matičnoj publikaciji
Light Metals 2016
Williams, Edward
Hoboken (NJ): John Wiley & Sons
978-1-119-22579-9
Podaci o skupu
TMS 2016 145th Annual Meeting & Exhibition:
predavanje
14.02.2016-18.02.2016
Nashville (TN), Sjedinjene Američke Države