The Inorganic Compounds of Iron and Nickel in Temperature Treated Synthetic Metallurgical Cokes
The iron and nickel content and the types of their inorganic compounds in metallurgical coke prepared with coal tar pitch as additive were investigated. Obtained synthetic coke samples were temperature treated up to 2400 C. The heating rate was 10 C/min, and heating time 2 and 4 hours. The results obtained showed that during temperature treatment the content of investigated metals is decreased.
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
Podaci o prilogu
207-x.
2000.
objavljeno
Podaci o matičnoj publikaciji
Sažeci predavanja s 4. međunarodnog simpozija hrvatskih metalurga, tiskano u Metalurgija 39(2000)3, 191-224
Mamuzić, Ilija
Zagreb: Hrvatsko metalurško društvo
Podaci o skupu
4. međunarodni simpozij hrvatskih metalurga
poster
25.06.2000-29.06.2000
Opatija, Hrvatska