Fatigue Strength of the Rolls with Grooves (CROSBI ID 201430)

Prilog u časopisu | izvorni znanstveni rad | međunarodna recenzija

Domazet, Željko ; Lukša, Francisko ; Bugarin, Miro Fatigue Strength of the Rolls with Grooves // Applied Mechanics and Materials, 459 (2014), 330-334. doi: 10.4028

Podaci o odgovornosti

Domazet, Željko ; Lukša, Francisko ; Bugarin, Miro

engleski

Fatigue Strength of the Rolls with Grooves

In “Steelworks Split” failures of the rolls with grooves on the 3-high-roughing mill stand occurred four times. Detailed analysis of all the elements which influenced the failure was carried out. Stress analysis shownthatthe most critical area of the roll is the 7.a caliber what is corresponding with fracture positions. The fatigue strength of the material in the caliber groove for fatigue life prediction was missing and fatigue strength is determined by experimental testing.

Fatigue strength; Hot rolling; Rolls with grooves

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

Podaci o izdanju

459

2014.

330-334

objavljeno

1660-9336

1662-7482

10.4028

Povezanost rada

Strojarstvo