Corrosion stability of welded alloy for metal- ceramic system
Objectives: The aim of this study was to test the elution of Co, Cr and Ni ions from laser and TIG welded Co-Cr alloys. Methods: Four commercial Co- Cr dental alloys were cast. The specimens were divided into 3 groups. The first group of samples was laser welded, second joint with TIG procedure and third used as a control group. After microstructure analysis the specimens were subjected to immersion test. Elution was determined using the AAS. Results: The highest leaching of the ions was shown for the specimens joined by TIG procedure. Statistically significant differences in the elution of Ni ions were recorded between all three analyzed specimen groups. The release of ions from analyzed specimens corresponds to their composition declared by the manufactures. Conclusions: Laser welds proved to be the most corrosion resistant, whereas TIG welds showed the highest ion elution.
Alloys; Corrosion; Lasers and Welding
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
Podaci o prilogu
228-228.
2012.
objavljeno
Podaci o matičnoj publikaciji
PER/IADR Helsinki ; abstracts ; u: Journal of Dental Research 91 (S.I. C)
Giannobile, William
Helsinki: International Association for Dental, Oral, and Craniofacial Research (IADR)
2231-2349
Podaci o skupu
PER/IADR Helsinki 2012
poster
12.09.2012-15.09.2012
Helsinki, Finska