Fracture of Jaw Arm Made of Cast Steel GS-42CrMo4 (CROSBI ID 577105)
Prilog sa skupa u zborniku | izvorni znanstveni rad | međunarodna recenzija
Podaci o odgovornosti
Smoljan, Božo ; Iljkić, Dario ; Tomašić, Neven ; Traven, Furio
engleski
Fracture of Jaw Arm Made of Cast Steel GS-42CrMo4
Unsuitable mechanical behaviour of cast steel GS-42CrMo4 (EN) was investigated. In this paper the influence of inclusions and pouring temperature on mechanical properties of arm of carrying jaw made of cast steel GS-42CrMo4 (EN) was investigated. It was found out that high content of aluminium caused the formation of aluminium nitride, AlN which significantly decreased strength of casting. In the process of solidification enrichment of lamellas of AlN nitride arise on the grain boundaries. Because of low deformability of AlN nitride, initiation of fracture was possible at minimal deformation. The strength of the casting was not being raised by subsequent heat treatment. High pouring temperature and low cooling rates resulted in coarse-grained microstructure of steel casting. Coarse microstructure was not being reduced by subsequent heat treatment.
cast steel; microstructure; mechanical properties
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
Podaci o prilogu
2010.
objavljeno
Podaci o matičnoj publikaciji
Proceedings of the International conference “Mechanical Technology and Structural Materials”
Podaci o skupu
International conference “Mechanical Technology and Structural Materials”
predavanje
21.10.2010-22.10.2010
Split, Hrvatska