Surface morphology of Cu-Al-Ni shape memory alloy after corrosion testing in 0.5 M NaCl solution (CROSBI ID 572097)

Prilog sa skupa u zborniku | izvorni znanstveni rad | međunarodna recenzija

Gojić, Mirko ; Kožuh, Stjepan ; Vrsalović, Ladislav ; Gudić, Senka ; Kliškić, Maja Surface morphology of Cu-Al-Ni shape memory alloy after corrosion testing in 0.5 M NaCl solution // Proceedings of XIII YuCorr International Conference / Pavlović, Miomir ; Lačnjevac, Časlav (ur.). Beograd: Savez inženjera Srbije za zaštitu materijala, 2011. str. 384-391

Podaci o odgovornosti

Gojić, Mirko ; Kožuh, Stjepan ; Vrsalović, Ladislav ; Gudić, Senka ; Kliškić, Maja

engleski

Surface morphology of Cu-Al-Ni shape memory alloy after corrosion testing in 0.5 M NaCl solution

Shape memory alloys are usable in numerous areas. The effect of the shape memory alloys is basically a recollection on a former deformation of the applied form of the material. In the physical sense, it is a byproduct of the martensite phase transformation in the structure of the homogenous matter. Microstructural analysis of Cu-Al-Ni alloy before corrosion testing was carried out by optical and scanning electron microscopy, respectively. The corrosion behaviour of Cu-Al-Ni shape memory alloy in deaerated 0.5 M NaCl solution at 20 ºC was studied by means of polarization measurements. Surface morphologies of selected specimens after corrosion testing (at -0.2V and 0.4V) were investigated by optical microscope, SEM and EDX microanalysis. The polarization measurements have shown that the corrosion behaviour of Cu-Al-Ni alloy in NaCl solution was dominated by the Cu component. The SEM and EDX microanalysis showed the presence of copper, aluminium and nickel oxides and chlorides on alloy surface.

shape memory alloy ; polarization ; corrosion ; microstructure

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

Podaci o prilogu

384-391.

2011.

objavljeno

Podaci o matičnoj publikaciji

Proceedings of XIII YuCorr International Conference

Pavlović, Miomir ; Lačnjevac, Časlav

Beograd: Savez inženjera Srbije za zaštitu materijala

978-86-82343-15-8

Podaci o skupu

XIII YUCORR International conference

poster

05.04.2011-08.04.2011

Tara, Srbija

Povezanost rada

Kemijsko inženjerstvo, Metalurgija