Cathodic breakdown of anodic oxide film on Al and Al-Sn alloys in NaCl solution
Cathodic breakdown of anodic oxide film on Al and Al-Sn alloys in NaCl solution // Electrochimica Acta, 50 (2005), 28; 5624-5632 (međunarodna recenzija, članak, znanstveni)
CROSBI ID: 149109 Za ispravke kontaktirajte CROSBI podršku putem web obrasca
Naslov
Cathodic breakdown of anodic oxide film on Al and Al-Sn alloys in NaCl solution
Autori
Gudić, Senka ; Radošević, Jagoda ; Smoljko, Ivana ; Kliškić, Maja
Izvornik
Electrochimica Acta (0013-4686) 50
(2005), 28;
5624-5632
Vrsta, podvrsta i kategorija rada
Radovi u časopisima, članak, znanstveni
Ključne riječi
Alminium; Aluminium activation; Al-Sn alloy; Anodic oxide film; Cathodic polarization
Sažetak
Influence of cathodic polarization on stability of defined oxide films on Al and Al-Sn alloys (with up to 0.40%Sn) has been investigated in a 0.5 M NaCl solution using the potentiostatic pulse method. The dependence of the cathodic current on time (in the period of 1, 10 and 100 s) were recorded on Al and Al-Sn alloys when subjected to a potential pulse from EOCP to different negative values (up to -2.0 V). Anodic current responses to the returned to the EOCP were also recorded at three different time scales (1, 10 and 100 s). It has been estabished that cathodic polarization of passivated Al and Al-Sn alloys in chloride solution is characterized by two regions of potentials with distinctly different phenomena: the range of low and high cathodic potentials (LCP and HCP). In LCP range oxide film retains its properties, while in the HCP range cathodic breakdown and hydration of the oxide take place. The boundary between these two potential ranges shifts towards more negative potential values when the % of Sn in the alloy increases. The longer the time of cathodic pulse, the more positive the potentials at which the oxide film breakdown takes place. This shift is more marked with alloys containing higher % of Sn. Cathodic polarisation (duration of 100 s) activates alloys with 0.20 and 0.40 % Sn for anodic dissolution.
Izvorni jezik
Engleski
Znanstvena područja
Kemijsko inženjerstvo
Citiraj ovu publikaciju:
Časopis indeksira:
- Current Contents Connect (CCC)
- Web of Science Core Collection (WoSCC)
- Science Citation Index Expanded (SCI-EXP)
- SCI-EXP, SSCI i/ili A&HCI
- Scopus
Uključenost u ostale bibliografske baze podataka::
- Chemical Abstracts
- APOLLIT
- BIOSIS
- Current Technology Index
- Elsevier BIOBASE
- Engineering Index
- Environmental Periodicals Library
- PASCAL/CNRS
- Scopus
- Zn/Pb/Cd Abstracts