Nalazite se na CroRIS probnoj okolini. Ovdje evidentirani podaci neće biti pohranjeni u Informacijskom sustavu znanosti RH. Ako je ovo greška, CroRIS produkcijskoj okolini moguće je pristupi putem poveznice www.croris.hr
izvor podataka: crosbi

Anomalous high-temperature oxidation in the zirconium-copper system (CROSBI ID 104604)

Prilog u časopisu | izvorni znanstveni rad | međunarodna recenzija

Paljević, Matija ; Tudja, Marijan Anomalous high-temperature oxidation in the zirconium-copper system // Corrosion science, 46 (2004), 2055-2065-x

Podaci o odgovornosti

Paljević, Matija ; Tudja, Marijan

engleski

Anomalous high-temperature oxidation in the zirconium-copper system

The high-temperature oxidation of the Zr-3 mass % Cu alloy and Zr2Cu in oxygen is characterized by selective oxidation of zirconium while the excess of copper is accumulated at the alloy-oxide interface forming the Zr8Cu5 phase. The oxidation of Zr2Cu at elevated temperatures shows an anomalous decrease of the oxygen consumption rate in the temperature range 890-975 °C. The oxide layer consists of monoclinic ZrO2 mainly, with preferentially oriented crystallites in depth region at 900 °C and tetragonal ZrO2 on the surface below 600 °C, and small amounts of CuO and Cu2O. The reaction kinetics obeys a parabolic rate law. The activation energy of 117.5 kJ/mol and 54.4 kJ/mol has been estimated for the oxidation of the Zr-3 mass % Cu alloy and Zr2Cu, respectively.

Zirconium-copper alloys; High temperature corrosion

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

Podaci o izdanju

46

2004.

2055-2065-x

objavljeno

0010-938X

Povezanost rada

Kemija

Indeksiranost