Analysis of a Pure Magnesium Membrane Degradation Process and Its Functionality When Used in a Guided Bone Regeneration Model in Beagle Dogs (CROSBI ID 308857)

Prilog u časopisu | izvorni znanstveni rad | međunarodna recenzija

Patrick Rider, Željka Perić Kačarević, Akiva Elad, Daniel Rothamel, Gerrit Sauer, Fabien Bornert, Peter Windisch, Dávid Hangyási, Balint Molnar, Bernhard Hesse and Frank Witte Analysis of a Pure Magnesium Membrane Degradation Process and Its Functionality When Used in a Guided Bone Regeneration Model in Beagle Dogs // Materials, 3106 (2022), 1-12. doi: 10.3390/ma15093106

Podaci o odgovornosti

Patrick Rider, Željka Perić Kačarević, Akiva Elad, Daniel Rothamel, Gerrit Sauer, Fabien Bornert, Peter Windisch, Dávid Hangyási, Balint Molnar, Bernhard Hesse and Frank Witte

engleski

Analysis of a Pure Magnesium Membrane Degradation Process and Its Functionality When Used in a Guided Bone Regeneration Model in Beagle Dogs

For the surgical technique of guided bone regeneration (GBR), the choice of available barrier membranes has until recently not included an option that is mechanically strong, durable, synthetic and resorbable. The most commonly used resorbable membranes are made from collagen, which are restricted in their mechanical strength. The purpose of this study is to evaluate the degradation and regeneration potential of a magnesium membrane compared to a collagen membrane. In eighteen beagle dogs, experimental bone defects were filled with bovine xenograft and covered with either a magnesium membrane or collagen membrane. The health status of the animals was regularly monitored and recorded. Following sacrifice, the hemimandibles were prepared for micro-CT (μ-CT) analysis. Complications during healing were observed in both groups, but ultimately, the regenerative outcome was similar between groups. The μ-CT parameters showed comparable results in both groups in terms of new bone formation at all four time points. In addition, the μ-CT analysis showed that the greatest degradation of the magnesium membranes occurred between 1 and 8 weeks and continued until week 16. The proportion of new bone within the defect site was similar for both treatment groups, indicating the potential for the magnesium membrane to be used as a viable alternative to collagen membranes. Overall, the new magnesium membrane is a functional and safe membrane for the treatment of defects according to the principles of GBR.

NOVAMag membrane ; resorbable membrane ; GBR ; healing ; magnesium degradation ; micro-CT

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

Podaci o izdanju

3106

2022.

1-12

objavljeno

1996-1944

10.3390/ma15093106