Corrosion behavior of copper, tin, and bronze CuSn14 in acid rain solution (CROSBI ID 300012)

Prilog u časopisu | izvorni znanstveni rad | međunarodna recenzija

Martinović, Ivana ; Pilić, Zora Corrosion behavior of copper, tin, and bronze CuSn14 in acid rain solution // Materials and corrosion, 72 (2021), 1635-1642. doi: 10.1002/maco.202112470

Podaci o odgovornosti

Martinović, Ivana ; Pilić, Zora

engleski

Corrosion behavior of copper, tin, and bronze CuSn14 in acid rain solution

The corrosion behavior of copper, tin, and bronze CuSn14 is studied in simulated acid rain (pH 4.5) by electrochemical techniques, cyclic voltammetry and electrochemical impedance spectroscopy. The potentiodynamic formation of anodic oxide film on copper and tin is described in terms of high‐field model. Cyclic voltammetry shows that dissolution of bronze is higher than of pure copper metal in acid rain. Electrochemical impedance spectroscopy data reveal that oxide films formed on copper and tin have a higher resistance and suppressed diffusion process through the surface layer than the oxide film formed on bronze CuSn14 at the same conditions.

bronze, copper, electrochemical methods, simulated acid rain, tin

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

Podaci o izdanju

72

2021.

1635-1642

objavljeno

0947-5117

1521-4176

10.1002/maco.202112470

Povezanost rada

Povezane osobe



nije evidentirano

Poveznice
Indeksiranost