Nalazite se na CroRIS probnoj okolini. Ovdje evidentirani podaci neće biti pohranjeni u Informacijskom sustavu znanosti RH. Ako je ovo greška, CroRIS produkcijskoj okolini moguće je pristupi putem poveznice www.croris.hr
izvor podataka: crosbi !

Corrosion Resistance of Open Die Forged Austenitic Stainless Steel Samples Prepared with Different Surfaces (CROSBI ID 295020)

Prilog u časopisu | izvorni znanstveni rad | međunarodna recenzija

Keran, Zdenka ; Stojanović, Ivan ; Horvatić Novak, Amalija ; Runje, Biserka ; Razumić, Andrej ; Vidovic, Denis Corrosion Resistance of Open Die Forged Austenitic Stainless Steel Samples Prepared with Different Surfaces // Sustainability, 13 (2021), 5871, 19. doi: 10.3390/su13115871

Podaci o odgovornosti

Keran, Zdenka ; Stojanović, Ivan ; Horvatić Novak, Amalija ; Runje, Biserka ; Razumić, Andrej ; Vidovic, Denis

engleski

Corrosion Resistance of Open Die Forged Austenitic Stainless Steel Samples Prepared with Different Surfaces

The use of corrosion-resistant metal materials in highly aggressive environments contributes to the preservation of the environment because it reduces the use of protective agents and coatings. Most metal objects are produced by some metal-forming process. It is well-known that plastic deformation affects the corrosion resistance of different metal materials in different ways. As a rule, austenitic stainless steels show a positive impact of plastic deformation on corrosion resistance, especially when hot deformed with protective surface oxide layers. However, most research carried out on these metals involves a carefully prepared surface which is either finely ground or polished. This paper investigates the corrosion resistance of cold-formed (open die forged) austenitic stainless steel in three different surface states for three different degrees of deformation. In doing so, we simulate possible damage to the treated surface and evaluate the stability of the material with respect to corrosion. Good corrosion resistance is shown for all three stages of deformation and for all three surface states, with some differences in the obtained results. Although the polished surface shows the highest corrosion resistance, as expected, the other two surfaces also demonstrate good results when exposed to aggressive environments. All of the results were statistically processed and presented. The results demonstrate the high usability of such materials in corrosion-aggressive environments with minimal danger of corrosion and minimal need to include additional surface protection agents, even against possible surface damage.

austenitic stainless steel ; corrosion resistance ; surfacing ; surface topography

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

Podaci o izdanju

13

2021.

5871

19

objavljeno

2071-1050

10.3390/su13115871

Povezanost rada

Strojarstvo

Poveznice
Indeksiranost